IEC 60404-5:1993
Magnetic materials - Part 5: Permanent magnet (magnetically hard) materials - Methods of measurement of magnetic properties
OVERVIEW
Applies to magnetically hard materials only. The described method makes use of a closed loop simulating a ring. Two alternative methods are given for intrinsic coercivity up to and including 600 kA/m and one for materials with higher intrinsic coercivity (e.g. rare earth cobalt alloys).
COMMENTS
-
PRODUCT DETAILS
| Status | Revised |
|---|---|
| Edition | 1993 |
| No. of Pages | 29 |
| ICS Classification | 29.030 Magnetic materials 17.220.20 Measurement of electrical and magnetic quantities |
| Committee | TC 68 |
| Available for Purchase | For sale in Singapore only |